Alloys 309 and 309S are austenitic chromium-nickel stainless steels that are often used for higher temperature applications. Due to their high chromium and nickel content, Alloys 309 and 309S are highly corrosion resistant, have outstanding resistance to oxidation, and excellent heat resistance while providing good strength at room and elevated temperatures. The only significant difference between 309 and 309S is the carbon content. Alloy 309S has a much less carbon composition which minimizes carbide precipitation and improves weldability.
Alloys 309 and 309S are used exclusively for their high temperature oxidation resistance, excellent high temperature strength, along with their resistance to creep deformation and environmental attack.
We are engrossed in the business of supplying and trading of premium quality 309 Stainless Steel Strip. Resistant to corrosion, the offered product is highly appreciated. Our team of quality controllers checks the whole range of products to be offered on various parameters thereby ensuring the durability and finishing of the products. Our offered product is customized as per client's requirements.
Used in Food Industries, Chemical Industries , Electrielcal Industries, Genrater Industries, Shaft Industries, Cement Industries, Gas Industries, Power Project etc..
| Standard | : | ASTM A240, ASME SA240 |
| Size | : | 1000 x 2000, 1220 x 2440, (4' x 8'), 1250 x 2500, 1500 x 3000 To 6000, 2000 x 4000 To 6000 | Thickness | : | 0.3 mm To 120 mm |
| C | Mn | Si | P | S | Cr | Ni | Fe | |
|---|---|---|---|---|---|---|---|---|
| 309 | max: 0.20 | 2.0 max | 0.75 max | 0.045 max | 0.03 max | min: 22.0 max: 24.0 | min: 12.0 max: 15.0 | Balance |
| 309H | min: 0.04 max: 0.10 | 2.0 max | 0.75 max | 0.045 max | 0.03 max | min: 22.0 max: 24.0 | min: 12.0 max: 15.0 | Balance |
| Grade | Tensile Strength ksi (min) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Brinell) MAX |
|---|---|---|---|---|
| 309/H | 40 | 30 | 40 | 217 |
| Density lbm/in3 |
Thermal Conductivity (BTU/h ft. °F) |
Electrical Resistivity (in x 10-6) |
Modulus of Elasticity (psi x 106 |
Coefficient of Thermal Expansion (in/in)/ °F x 10-6 |
Specific Heat (BTU/lb/ °F) |
Melting Range (°F) |
|---|---|---|---|---|---|---|
| at 68°F: 0.285 | 9.0 at 32- 212°F | 30.7 at 68°F | 28.5 | 8.28 at 32 – 212°F | 0.1200 at 68°F to 212°F | 2500-2590 |