NG Industries is a pioneer in Pure Titanium Gr 4 Plates Supplier and Titanium AMS 4902 Strips exporter, of the quality Titanium Grade 4 Sheets and Plates; having openness in a colossal scope of titanium and titanium alloy sheets and plates. Pure Titanium Grade 4 Sheets and Plates is a warmth treatable and has taking off pliability and quality close by with top notch fabricability and weldability. It's a gathering of uncommon great quality and corrosion resistance, demonstrating the most extreme quality of the greater part of the unalloyed evaluations. They are used in a range of chemical procedure paraphernalia in addition to in aeronautical and marine applications.
Pure Titanium Grade 4 Plates & Sheets is an unalloyed, standard quality titanium products. This titanium evaluation is utilized as a part of flying machine motors, marine and airframes parts, where it's recognizing qualities are corrosion resistance and great weldability. Working towards the point of customer fulfillment, we offer these items at the most reasonable industry costs.
Specifications :
| Grades |
Titanium GR-4
|
| Standard |
GB / T 3621 -44 , ASTM B 265, ASME SB 265 |
| Werkstoff Nr |
3.7035 |
| Thickness |
1mm – 100mm |
| Width |
1000mm – 3000mm |
| Production |
Hot-Rolled (HR) / Cold-Rolled (CR) |
| Application |
Chemicals & Fertilizers Industries , Sugar Mills , Cement Industries , Ship Building , Paper Industries , Oil & Gas , Petrochemicals , etc |
Chemical Composition :
|
C |
Fe |
H |
N |
O |
Ti |
|
max |
max |
max |
max |
max |
max |
|
0.1 |
0.3 |
0.015 |
0.03 |
0.25 |
99.2 |
Mechnical Properties :
| Hardness, Knoop | 170 | 170 | |
| Hardness, Rockwell B | 80 | 80 | |
| Hardness, Vickers | 145 | 145 | |
| Tensile Strength, Ultimate | 344 MPa | 49900 psi | |
| Tensile Strength, Yield | 275 - 410 MPa | 39900 - 59500 psi | |
| Elongation at Break | 20 % | 20 % | |
| Reduction of Area | 35 % | 35 % | |
| Modulus of Elasticity | 105 GPa | 15200 ksi | In Tension |
| Compressive Modulus | 110 GPa | 16000 ksi | |
| Poisson's Ratio | 0.37 | 0.37 | |
| Izod Impact | 114 - 171 J | 84.1 - 126 ft-lb | |
| Fatigue Strength | 300 MPa | 43500 psi | 1E+7 cycles, Unnotched |
| Fatigue Strength | 425 MPa | 61600 psi | 30,000 cycles, Unnotched |
| Fracture Toughness | 66 MPa-m½ | 60.1 ksi-in½ | K(Q); annealed |
| Shear Modulus | 45 GPa | 6530 ksi | |